2002 Ford Excursion 2WD V10-6.8LFACTORY OEM SERVICE PROCEDURE

Transmission and Drivetrain: Service and Repair

Axle Housing Casting Porosity (Holes in Casting) Repair

NOTE: Do not disassemble the carrier. Make repairs on the outside of the axle.

NOTE: Casting porosity is a condition where occasionally gas bubbles will form during the casting process leaving small pockets in the metal that may cause the axle housing to show signs of dampness.

Factory service manual diagram




1. To fill small pockets, peon in a small amount of body lead.
2. Seal the pocket.
- Use Devcon Aluminum Liquid F2 or equivalent meeting Ford specification M-3D35A (E).
3. To fill large pockets, drill and tap a shallow hole for a small setscrew. Install the setscrew and seal it.
- Use Devcon Aluminum Liquid F2 or equivalent meeting Ford specification M-3D35A (E).
Factory Service Tools

Use the Manual With the Right Hardware

Pair factory procedures with proven DIY tools so the instructions are easier to execute.

Disclosure: Verified tool recommendations may earn an affiliate commission at no cost to you.

When to See a Mechanic

Stop DIY work and contact a certified mechanic immediately if any of the following apply:

  • β€’ You smell fuel, burning insulation, or see smoke.
  • β€’ Brakes feel soft, pull hard to one side, or make grinding noises.
  • β€’ The engine overheats, stalls repeatedly, or misfires under load.
  • β€’ You are missing required tools, torque specs, or safe lifting equipment.
  • β€’ You are not confident in the next step or safety outcome.